Code

ISO 5817: quality levels B, C, and D for imperfections in steel welds.

The international standard that sets three quality levels for imperfections in fusion welds of steel, nickel, and titanium, and that every ISO weld acceptance standard hangs off.

Welding — Fusion-welded joints in steel, nickel, titanium and their alloys — Quality levels for imperfections · ISO · ISO 5817:2023

What it covers

ISO 5817 in plain terms.

ISO 5817 is the quality book for fusion welds in steel, nickel, titanium, and their alloys. It names each imperfection by its ISO 6520-1 number and sets, for each, what is allowed at three quality levels: B, the most stringent; C, intermediate; and D, moderate. Beam welding is out, because ISO 13919 covers it, and aluminum has its own standard in ISO 10042.

The quality level is a design decision. The application standard, the contract, or the designer picks it from the loads, the consequences of failure, and the cost of making the weld, and it can differ from weld to weld on the same structure. In Europe EN 1090-2 ties the level to the execution class of a steel structure, and the welder and procedure qualification standards use it to judge test pieces.

ISO 5817 does not say how to look. Each NDT method has its own acceptance standard that turns the quality level into limits for what that method can see: ISO 10675 for radiography, ISO 11666 for ultrasonic testing, ISO 23277 for penetrant testing, and ISO 23278 for magnetic particle testing. Visual testing to ISO 17637 is judged directly against ISO 5817, because a surface imperfection can be measured the way the standard describes it. ISO 17635 gives the general rules that tie the methods to the levels.

The limits describe the weld as made, before any repair, and they are not a target: a weld at quality level D is a sound weld for the duty it was chosen for. An annex adds requirements for structures under fatigue, where the shape of the weld matters more than it does under static load.

In the glossary: Acceptance criteria · Imperfection · Quality level

Regulation

In Europe EN 1090-2 picks the ISO 5817 quality level from the execution class of a steel structure, and ISO 15614-1 and ISO 9606-1 judge procedure and welder test pieces against it.

Full title
Welding — Fusion-welded joints in steel, nickel, titanium and their alloys — Quality levels for imperfections
Issued by
ISO, adopted in Europe as EN ISO 5817
Current edition
ISO 5817:2023
Applies to
Fusion welds in steel, nickel, titanium, and their alloys; beam welding is covered by ISO 13919 and aluminum by ISO 10042
Quality levels
B, the most stringent; C, intermediate; D, moderate
Imperfection names
ISO 6520-1 names and reference numbers
Acceptance standards built on it
ISO 10675 for radiography, ISO 11666 for ultrasonic testing, ISO 23277 for penetrant testing, and ISO 23278 for magnetic particle testing
Visual testing
ISO 17637, judged directly against ISO 5817

Who it's for

One record. Both sides of the job.

How inspection works

Methods under ISO 5817.

Who sets the procedure, who sets acceptance, and who may do the work, method by method.

MethodProcedureAcceptanceCertification
Visual (VT)ISO 17637ISO 5817 at quality level B, C, or DISO 9712 VT Level II, or a certified welding inspector
Radiographic (RT)ISO 17636ISO 10675 at the acceptance level that matches the quality levelISO 9712 RT Level II
Ultrasonic (UT)ISO 17640ISO 11666 at the acceptance level that matches quality level B or CISO 9712 UT Level II
Magnetic particle (MT)ISO 17638ISO 23278 at the acceptance level that matches the quality levelISO 9712 MT Level II
Penetrant (PT)ISO 3452-1ISO 23277 at the acceptance level that matches the quality levelISO 9712 PT Level II

Acceptance criteria

How a weld passes or fails.

Each imperfection type has its own limit at each quality level, and the limits tighten from quality level D to quality level B.

  • Cracks are not permitted at any quality level.
  • Porosity is judged by the size of each pore and by how much of a reference area the pores take up, with clusters and lines of pores judged on their own.
  • Undercut, excess weld metal, excess penetration, and misalignment are judged by their dimensions against the material thickness.
  • Lack of fusion and incomplete penetration are limited or not permitted, depending on the quality level.
  • Imperfections that repeat along a weld, and several imperfections in one cross section, are judged together, not one at a time.

Which of these an NDT method can find, and to what limit, is the job of that method's acceptance standard, not of ISO 5817.

A summary, not the code. Limits and exceptions are in the edition your job works to.

The report

What ISO 5817 reports have to carry.

The fields a Level III checks before signing. Miss one and the report comes back.

  • Weld and component ID, material, and thickness
  • ISO 5817 quality level for the weld, and who set it
  • The method and its technique standard, and the acceptance standard and level used for that method
  • Each imperfection: ISO 6520-1 name and reference number, location, and size
  • Accept or reject per imperfection and per weld
  • Repairs and the retest that followed them
  • Technician name, certification, and date

How Weld Done builds your NDT report template

Standards logic

Checked at capture, not after the report.

Where Weld Done holds a code's acceptance limits, each RT, VT, and UT indication is checked against them as it's entered. A rejected one shows the clause, the value, and the limit.

Standards logic →
  1. No quality level on the job.

    Without it, no acceptance level can be chosen for any method, and the report can only describe what was found.

  2. Quality level B asked for everywhere.

    The level is meant to follow the duty of the weld. Asking for the most stringent level on every weld adds cost and repairs without adding safety where the loads do not call for it.

  3. Ultrasonic testing on a quality level D weld.

    ISO 11666 has no acceptance level for quality level D. The application standard has to say which method and which limits apply.

  4. Imperfections named in local terms.

    ISO 5817 and the acceptance standards speak in ISO 6520-1 numbers. A report that says only "porosity" cannot be checked against the limit for the kind of porosity found.

Related codes

The codes around it.

Edition referenced: ISO 5817:2023. All codes and standards

FAQ

Questions.

Every other answer is on the FAQ page.

Visit FAQ
What are ISO 5817 quality levels B, C, and D?

Three sets of limits for weld imperfections. Quality level B is the most stringent, C is intermediate, and D is moderate. The design picks the level from the duty of the weld.

Who chooses the ISO 5817 quality level?

The application standard, the contract, or the designer. In Europe EN 1090-2 ties it to the execution class of the structure.

How does ISO 5817 relate to ISO 10675, ISO 11666, ISO 23277, and ISO 23278?

ISO 5817 sets the quality level. Each of those standards turns it into an acceptance level for one NDT method: radiography, ultrasonic testing, penetrant testing, and magnetic particle testing in that order.

Does ISO 5817 cover aluminum?

No. ISO 10042 sets the quality levels for arc-welded aluminum, and ISO 10675-2 judges its radiographs.

What changed in ISO 5817:2023?

The 2023 edition replaces the 2014 edition and its amendment. The three quality levels and the ISO 6520-1 naming stay; a Level III checks the detail of each limit against the current text.

See your own report rebuilt.

Book a 30-minute demo on one of your real reports.

Not ready to talk? The calculator works out hours and costs back from your own numbers.